Product Detail
Mechanical Properties
| Property |
Testing Method |
Testing Condition |
Injection Molding Typical Value |
3D Printing X-Y Axis Typical Value |
3D Printing Z Axis Typical Value |
Unit |
| Tensile Strength |
ISO 527 |
50mm/min |
53.8 |
53.1±4 |
26.2±2 |
MPa |
| Elongation at Break |
ISO 527 |
50mm/min |
49.5 |
2±0.5 |
1.2±0.2 |
% |
| Tensile Modulus |
ISO 527 |
50mm/min |
1490.1 |
1430±100 |
1217±100 |
MPa |
| Flexural Strength |
ISO 178 |
2mm/min |
76.9 |
74.1±4 |
30.9±4 |
MPa |
| Flexural Modulus |
ISO 178 |
2mm/min |
2266.7 |
2020±100 |
1780±100 |
MPa |
| Charpy Impact Strength |
ISO 179 |
23℃ |
NB |
13±2 |
5.8±1 |
KJ/㎡ |
| Izod Impact Strength |
ISO 180 |
23℃ |
NB |
9.3±2 |
5±1 |
KJ/㎡ |
Physical Properties
| Property |
Testing Method |
Testing Condition |
Typical Value |
Unit |
| Density |
ISO 1183 |
Immersion |
1.33 |
g/cm3 |
| Melt Flow index(MFR) |
ISO 1133 |
275℃/2.16kg |
10-20 |
g/10 min |
Moisture Absorption
| Property |
Testing Method |
Testing Condition |
Injection Molding Typical Value |
3D Printing Typical Value |
Unit |
| Moisture Absorption |
ISO 62 |
50%RH*23℃ |
0.4 |
0.42 |
% |
Chemical Properties
| Property |
Testing Result |
| Weak Acid Resistance |
Lightly Resistant |
| Strong Acid Resistance |
Not Resistant |
| Weak Base Resistance |
Lightly Resistant |
| Strong Base Resistance |
Not Resistant |
| Oil and Grease Resistance |
Resistant |
Thermal Properties
| Property |
Testing Method |
Testing Condition |
Injection Molding Typical Value |
3D Printing X-Y Axis Typical Value |
3D Printing Z Axis Typical Value |
Unit |
| Glass Transition Temperature |
DSC |
10℃/min |
83.7 |
℃ |
| Crystallization temperature |
DSC |
10℃/min |
150 |
℃ |
| Melting Point |
DSC |
10℃/min |
244.1 |
℃ |
| Distortion Temperature |
TGA |
20℃/min |
N/A |
℃ |
| Heat Distortion Temperature |
ISO 75 |
0.45MPa |
72.3 |
70.1 |
68.6 |
℃ |
| Heat Distortion Temperature |
ISO 75 |
1.8MPa |
63.8 |
60.6 |
58.8 |
℃ |
| Vicat Softening Temperature |
ISO 306 |
50℃/10N |
82.4 |
79.3 |
76.1 |
℃ |
Recommended 3D Printing Parameters*Based on 0.4 mm nozzle. Printing conditions may vary with different nozzle diameters.
| Printing Temperature |
250-280(℃) |
| Bed Temperature |
70-90(℃) |
| Wall Layers |
2 Layers |
| Top and Bottom Layers |
4 Layers |
| Infill |
100% |
| Ambient Temperature |
25℃ |
| Cooling Fan |
0-10% |
| Printing Speed |
30-50 (mm/s) |
| Nozzle Diameter |
0.4 mm |